Saturday, April 11, 2026

Archives

March 2026

Simulation-based prediction of the thermal process emission measured by pyrometry of 316L stainless steel

Laser powder bed fusion is a common additive manufacturing process in which metal powder is selectively melted by a laser. Meandering stripe hatching is often used in conjunction with constant process parameters such as laser power and scan speed. However, the exposure strategy and the part geometry influence the resulting melt pool. To compensate for […]
Tobias Baranzke, Sebastian Bremen, Florian Eibl

Effect of various heat-treatment methods on AISI 4140 steel

AISI 4140 steel is one of the important categories in the steels with a wide range of applications including but not limited to automotive, general machinery, and the oil and gas industry. In the current study, an effort is made to understand the effects of heat-treatment parameters, such as heat-treatment temperature and holding time, on […]
Sharan Mudda, Sathyashankara Sharma, B. M. Gurumurthy, M. C. Gowrishankar, Ananda Hegde, Manjunath Shettar

February 2026

Efficiency and evolution: How modern burners are redefining industrial combustion

Industrial combustion systems remain at the heart of process heating across manufacturing, energy generation, and infrastructure. As energy prices fluctuate and environmental standards tighten, burner technology has quietly evolved into a high-precision field where control, safety, and sustainability must coexist. In the U.K. and across Europe, companies such as Dunphy Combustion have spent decades refining […]
James Kuligowski, MEng

High temp insulation: Versatile and efficient ceramic fiber solution

High-temperature insulation is a critical component in industrial thermal processing, maximizing efficiency, reducing energy costs, and extending equipment lifespan. As industries seek increasingly effective solutions, the demand for specialized thermal insulation is growing rapidly. This article will explore the benefits of high-temperature insulation, focusing on ceramic fiber products. It will analyze their properties, key applications, […]
Jonathan Whaley

January 2026

The effects of deep cryogenic treatment on M2 high speed steel

Deep cryogenic treatment has been reported to be a beneficial process for improving the properties and microstructure of steels. Generally, deep cryogenic treatment should be combined with tempering to achieve the optimal effects on steels. However, the microscale relationship between deep cryogenic treatment and subsequent tempering is unclear. Therefore, the effects of deep cryogenic treatment […]
Zeju Weng, Kaixuan Gu, Chen Cui, Mingli Zhang, Liubiao Chen, Junjie Wang

Preventing discoloration in vacuum heat treatment: Guidelines for contamination control

Discoloration in vacuum heat treatment can indicate contamination, leading to potential product quality issues and process inefficiencies. Even minor contamination can compromise part integrity, causing oxidation, residue buildup, and surface defects. This article explores the key sources of contamination in vacuum furnaces, including outgassing, backstreaming, leaks, and particle generation. Learn how to identify, evaluate, and […]
Janusz Kowalewski