Tenova LOI Thermprocess gets order for installation of thin plate quench

0
2273
The Tenova LOI Thermprocess quench is designed for efficient cooling of thin and very thin plates of high strength and wear-resistant material. (Courtesy: Tenova LOI Thermprocess)

Tenova LOI Thermprocess has received another order from Wuhan Iron & Steel Co. Ltd. (WISCO) for the installation of a continuous quench for efficient cooling of thin steel plates.

The Tenova LOI Thermprocess quench is specially designed for efficient cooling of thin and very thin plates of high strength and wear-resistant material. The quenches adopted for this application ensure maximum hardness and outstanding flatness combined with unique and powerful models and overall automation.

For Tenova LOI Thermprocess, a leading global company in the field of heat treatment plants, it is the fourth order from Wuhan Iron & Steel in the field of plate heat treatment. This additional contract points out the successful, long-term cooperation of the two companies for this business, which started in 1994.

In addition to the previously installed equipment for treating medium and thick plates, the new quench extends WISCO’s capabilities for thin plate heat treatment.