SECO/WARWICK Allied Pvt. Ltd. has installed single chamber vacuum hardening furnace with high pressure gas quenching facility for Jyoti Heat Treat Industries

0
1085

The Vector™line furnace with high-pressure gas quench facility is ideally suitable for Vacuum Hardening in an oxygen free environment. Heating can be performed in vacuum as well as under convection with partial pressure. Quench pressure can be adjusted from 1.5 bar to a maximum of 10 bar. The Vector furnace installed at Jyoti can also be used for additional processes such as vacuum annealing, normalizing & tempering. The furnace has effective uniform hot zone size of 600x600x900 mm (24”x24”x36”) & load capacity of 600 Kgs (1320 lbs.). The furnace complies with NADCA requirement and is equipped with an advanced PLC/HMI control system.

For more information on Jyoti Heat Treat Industries, contact the company by phone at +91 20 2712 8944.

For additional information on the SECO/WARWICK Group, go to www.secowarwick.com.