Going viral: Outside-the-box research into sterilizing N95 masks for re-use
With the COVID-19 pandemic still raging across the country and the world, the need for personal protective equipment for medical […]
Nonlinear electromagnetic acoustic testing method for tensile damage evaluation
This paper describes an approach for measuring material plasticity using contactless electromagnetic acoustic method. Harmonic generation from noncumulative fundamental longitudinal […]
Q&A with Jeff Marshall
What does MHV do for the heat-treat industry? We make our customers more competitive, which is good both for the […]
Abbott Furnace Company
Abbott Furnace Company is an industrial furnace manufacturer with more than 35 years of experience designing and producing some of […]
Advanced Energy Industries Inc.
Advanced Energy shapes and transforms how power is used, delivered, and managed. Advanced Energy has devoted decades to perfecting power […]
Aerospace Testing and Pyrometry
Aerospace Testing & Pyrometry, Inc. specializes in the onsite calibration of temperature processing instrumentation, calibration of vacuum measuring systems and […]
AFC-Holcroft
AFC-Holcroft has one of the most diversified product lines in the heat treat equipment industry. We are fully equipped to […]
Air & Energy Systems
For over 40 years Air & Energy Systems has provided high quality heat processing equipment to a large variety of […]
Air Products
Air Products touches the lives of consumers around the globe in positive ways every day. Focused on serving energy, environment […]
Ajax Tocco Magnethermic Corporation
Ajax TOCCO Magnethermic®, a subsidiary of ParkOhio Holdings Corp.®, designs and manufactures world-class induction heating and melting equipment for various […]
Ambrell Induction Heating Solutions
Ambrell Corporation is a global leader in the induction heating market. We are headquartered in the United States with operations […]
Applied Test Systems
Applied Test Systems is a leading manufacturer of materials testing & process heating equipment.
Arrow Tank & Engineering Company
Arrow Tank and Engineering is a fabricator of pressure vessels – ASME, custom machinery and weldments. We have two direct […]
Axim Mica
From high temperature mica insulation sheets to flexible mica composites, Teflon, mica flakes for sale, find at Axim Mica.
BASF Metals LLC, Temperature Sensing
BASF has consistently advanced temperature measurement in the glass industry for more than 60 years.
Blasdel
Leading designer and manufacturer of industrial infrared ovens.
C3 Data
C3 is a software platform built specifically for the thermal processing industry to help ensure furnace compliance to any number […]
Can-Eng Furnaces International Ltd.
There really is no standard furnace. Our strength is the ability to custom engineer a furnace for any customer requirement. […]
CEIA USA Ltd
CEIA SPA is a leading manufacturer and designer of Medium to High frequency induction heating units. Throughout its history, the […]
Centorr Vacuum Industries
Centorr Vacuum Industries is a manufacturer of high temperature vacuum and controlled atmosphere furnaces.
CeraMaterials
CeraMaterials is a global manufacturing, distribution, design and sales organization specializing in high temperature refractory materials including carbon, graphite, CFC, […]
CHE Furnaces
CHE was established in 1988 and has over 80 years combined staff experience in manufacturing industrial furnaces for the Aerospace, […]
Conax Technologies
Conax Technologies is a leader in the design and manufacture of temperature sensors, compression seal fittings, and cable and harness […]
Conrad Kacsik Instrument Systems Inc.
Conrad Kacsik Instrument Systems distributes, services, system engineers and provides certified calibration for process control instrumentation and process control systems. […]
Cyprium Induction
We’re committed to providing you with the highest level of service, so you’ll always be happy that you chose us. […]
DMP CryoSystems
DMP CryoSystems has been in the manufacturing business for two decades. We are a family owned and operated business that […]
Dry Coolers Incorporated
We engineer and manufacture industrial cooling systems in Oxford, Michigan, USA.
East Carolina Metal Treating, Inc.
Service is our business and making sure our customers’ expectations are exceeded is our top priority. We have set up […]
ECM USA, Incorporated
Our mission is to provide high quality vacuum furnaces, services and spare parts to our North American customer base for […]
Epcon Industrial Systems LP
Founded in 1977, Epcon has grown from a one man-operation to a global leader in developing and manufacturing innovative air […]
Eurotherm by Schneider Electric
Our wide range of products is rich in features and designed for easy operation and reduced engineering time. They contain […]
Furnace Brokers Incorporated
Walk-in ovens, cabinet ovens, heat treat furnaces, vacuum furnaces, and internal oil quench furnaces.
Gasbarre Thermal Processing Systems
Gasbarre Thermal Processing Systems designs, manufactures and services a full line of heat treating equipment for virtually any process. Gasbarre’s […]
Gefran
Gefran offers precision devices for measuring process variables: temperature, power, pressure and position. The primary elements are produced in clean […]
Graphite Insulation
Graphite Insulation Mission Statement GraphiteInsulation.com is an e-commerce platform for engineers, maintenance managers, and procurement offices to research, purchase and […]
HeatTek, Inc.
Specialized in Custom Industrial Ovens, Furnaces, & Washers HeatTek is the only thermal equipment supplier that delivers complete confidence every […]
Advanced Flame Hardening Incorporated
Adesso Precision Machine Company
Advanced Energy Industries Inc.
Advanced Heat Treat Corp. – Cullman
Advanced Heat Treat Corp. – Monroe
Advanced Heat Treat Corp. – Waterloo
Advanced Surface Technologies Inc.
Aerospace Testing and Pyrometry
Agilent Technologies Vacuum Products
Aichelin Heat Treatment Systems Inc.
Ajax Tocco Magnethermic Corp. – Detroit