Archives
August 2025
ARTICLES
The effect of heat treatment and cold forging on the mechanical properties of SCr420 low-alloy steel
This study developed a new heat treatment method, normalizing and stress relief (NSR), to increase productivity compared to spheroidizing annealing (SA). The influence of different microstructures resulting from these heat treatments was investigated in cold-forged steel. Despite a shorter heat treatment time, the mechanical properties of the NSR alloy were found to be similar to […]
The Influence of induction hardening, nitriding, and boronizing on certain steels
Heat-treatment technology changes all the mechanical properties of metallic materials. The influence of induction hardening, nitriding, and boronizing on the change in the microhardness, impact toughness, microstructure, and coefficient of friction of conventional steels 42CrMo4 and 32CrMo12 has been examined and compared with results obtained in the sintered steels with an increased content of Cu, […]
NEWS
Seco/Warwick powers aircraft engine production
A premium manufacturer in the aviation industry has invested in an advanced vacuum furnace from Seco/Warwick for brazing fuel system components for aircraft engines. Seco/Warwick will deliver yet another vacuum furnace system for a manufacturer of components for aircraft engines. This is the result of years of collaboration with this partner. A single-chamber vacuum furnace with a […]
September 5, 2025
LK Metrology Ltd. acquires Procon X-Ray
LK Metrology Ltd., based in Castle Donington, UK, announced the acquisition of ProCon X-Ray GmbH, a specialist German manufacturer of computed tomography (CT) systems. LK Metrology is best known as a manufacturer and global supplier of coordinate measuring machines (CMMs) and, more recently, laser scanning sensors. With this strategic acquisition, LK Metrology broadens its portfolio […]
September 5, 2025
Nutec Bickley car bottom furnace headed for Midwest
Nutec Bickley recently gained an order for a gas-fired car bottom furnace for one of the most well-established heat–treat operations in the U.S .Midwest. This furnace will be capable of handling both steel and aluminum ingots and has been designed to operate across a wide temperature range. The high levels of temperature uniformity to be […]
September 5, 2025
Retech expands tolling services in melting, casting
Retech, a Seco/Warwick Group company, is expanding its toll melting, atomizing, and casting services to meet increasing demand across industries such as aerospace, medical, defense, and semiconductors. Retech is best known for designing and building custom systems for other companies, but it also maintains a suite of operational equipment at its Buffalo, New York, facilities. […]
September 5, 2025
Gruenberg ships conveyor oven to semiconductor industry
Gruenberg®, a leading manufacturer of industrial ovens and sterilizers, shipped a custom Gruenberg conveyor oven to the semiconductor industry for drying a specialized coating onto small parts. The electrically heated drying oven has a maximum temperature rating of 450°F and is configured with one heating module and one cooling module. The system uses high-volume […]
September 5, 2025
Advanced Heat Treat Corp. expands Michigan facility
Advanced Heat Treat Corp. (AHT), a recognized leader in heat treat services, has completed a 6,000-square-foot expansion at its Monroe, Michigan, facility. The climate-controlled addition will free up production space, provide an area for additional equipment and services, and includes new office space and a modern breakroom. Groundbreaking for the project took place on November […]
August 27, 2025
APMI International Names 2025 Fellows at June conference
The 2025 recipients of APMI International’s 2025 Fellow Award are Christopher Adam, PMT, president, Valimet, Inc., and Dr. Ma Qian, distinguished professor, Royal Melbourne Institute of Technology. The group’s most prestigious award recognizes APMI members for their significant contributions to the goals, purpose, and mission of the organization as well as for an elevated level […]
August 14, 2025
Somary named Ipsen USA CEO after McKenna steps down
Former Ipsen USA president and CEO Patrick McKenna has left the company to pursue another opportunity. Ipsen Group CEO Geoffrey Somary has assumed the responsibilities of Ipsen USA CEO. Somary will also continue in his role leading the global organization. “We would like to thank Patrick for his dedication and many contributions to Ipsen’s success […]
August 14, 2025
Seco/Warwick, USA has new director of sales for N. America
Seco/Warwick, USA recently announced Tom Hart has been promoted to director of sales for North America. With more than two decades of experience serving the precision manufacturing and heat-treatment technology sectors — underscored by his leadership in industry groups, including the American Gear and Manufacturing Association (vice-chair Materials and Metallurgy Committee, member of the Aerospace […]
August 14, 2025
Ipsen USA welcomes seven 2025 summer interns
Ipsen USA launched its 2025 Summer Internship Program, welcoming seven interns from regional universities to its Vacuum Technology Excellence Center. The interns — Payton C., Elija S., Logan A., Eli D., Ella C., Kennedy B., and Abigail J. — are engaging in hands-on roles across several departments, including engineering, marketing, controls, finance, human resources, and […]
August 14, 2025
Solar Manufacturing ships vacuum carburizing furnace
Solar Manufacturing recently shipped a large, state-of-the-art vacuum carburizing furnace to a prominent aerospace company known for producing advanced, high-precision components for the global aviation and aerospace engine industry. Headquartered in North America, the company’s aerospace division has been a trusted supplier to the aeroengine sector for decades, with manufacturing operations spanning the globe. To […]
August 14, 2025