Can-Eng to deliver furnaces to heat treat closed die forgings

0
1198
A Can-Eng cast link belt. (Courtesy: Can-Eng Furnaces International LTD)

Can-Eng Furnaces International LTD, has been contracted to deliver a significant number of different furnace types to multiple unique customers in the United States and Canada.

These furnaces are for the heating and heat treatment of both aluminum and steel closed die forgings. The furnace configurations either under construction in the company shops or in the early stages of commissioning include rotary hearth, chain conveyor, roller hearth, mesh belt, and cast link belt. The current uptick in activity from the forging sector represents a major portion of the company’s order backlog. These furnaces will be delivered to Georgia, North Carolina, and Ontario and will be used in the production of powertrain, suspension, and steering/linkage components for the automotive sector.

The demand for new state-of-the-art furnace equipment has been driven by both light weighting initiatives and a shortage of in-house heat-treatment capacity. All contracts will be in production by late Q1 2021.

MORE INFO  www.can-eng.com