Can-Eng to deliver second mesh belt furnace line

0
1585
Can-Eng Furnaces announced a contract to deliver a second mesh belt heat treatment furnace to a commercial heat treater. (Courtesy: Can-Eng Furnaces)

Can-Eng Furnaces International, Ltd. has recently been awarded a contract to deliver a second high-capacity mesh belt heat treatment furnace line to a commercial heat treater in the Midwest United States. Can-Eng completed commissioning of a 4,000 lb/hr mesh belt furnace system for this customer in 2020. With some run time on the new equipment, it was quickly realized that improvements in the Can-Eng designs — which include soft part handing, precision temperature + atmosphere control, energy efficiency, and reduction in oil drag out — not only were producing a higher quality part but doing so at a reduced operational costing.

This duplicate 4,000 lb/hr high-capacity mesh belt furnace line is to be installed alongside the previous furnace line in the recently expanded plant.

These custom-engineered continuous atmosphere heat-treating systems feature an increase in usable hearth area to provide high-volume processing when running products requiring carbon diffusion and lighter belt loading, as they will be used primarily for demanding processing including carbonitriding and carburizing. The furnaces are capable of a maximum throughput capacity of up to 4,000 lb/hr neutral hardening each.

Both furnace lines feature a computerized controlled automated bin dumping and vibratory part feeder system, dunk and spray pre-washer, protective atmosphere-controlled mesh belt hardening system, oil quench, dunk and spray post wash system, forced recirculation temper furnace, in-line post cooling system, and Can-Eng’s PETTM Level 2 SCADA system. By integrating Can-Eng’s Level 2 Automation, the end user has access to vital tracking of products’ status, detailed process data for continuous process improvements, comprehensive equipment diagnostics, cost analysis, and inventory management, which is required by many demanding customers.

This new line marks the fifth Can-Eng mesh belt furnace line to be in operation at the facility.

Can-Eng Furnaces International is a global provider and leader of state-of-the-art thermal processing systems. Headquartered in Niagara Falls, Ontario, Canada, Can-Eng is an ISO 9001:2015 certified company.