Can-Eng adding roller hearth iso-thermal annealing line in NC

0
1144
Installation of a Can-Eng roller hearth iso-thermal annealing line for an American producer of steel automotive impression forgings will begin in Q2 2024. (Courtesy: Can-Eng Furnaces International LTD)

Can-Eng Furnaces International LTD, has secured a contract for a roller hearth iso-thermal annealing line for an American producer of steel automotive impression forgings in North Carolina. 

The system will be capable of both iso-thermal annealing and normalizing consisting of a high-temperature furnace operating under EXO atmosphere, a separate low-temperature roller hearth furnace, automatic bin dump and loading system, integrated tray/basket return system, and level II automation technology. Installation of the equipment will begin in Q2 2024. This is the fourth contract awarded to Can-Eng in recent years; the previous three were configured as a mesh belt normalizing furnace, cast link belt normalizing furnace, and a roller hearth iso-thermal annealing furnace. 

MORE INFO  www.can-eng.com