Tenova wins another order in aluminum strip processing line by Henan Tongren

0
1666

Henan Tongren Aluminium Co. Ltd, gave Tenova a contract for a continuous annealing and chemical pretreatment line for processing strip coils for the aluminum market.

Henan Tongren Aluminium Co. Ltd is a Chinese manufacturer specializing in the production of aluminum products. Tenova is a company of the Techint Group specializing in innovative solutions for the metals and mining industries. The new contract for a continuous annealing and chemical pretreatment line will be realized in Sanmenxia, Henan Province, China. This totals more than fifteen references in China, North America, and Europe.

The new line will process automotive and aircraft aluminum alloys, family series 2XXX, 5XXX, 6XXX, and 7XXX, with a strip width range from 1.000 mm up to 2.650 and thickness range from 0.3 up to 4.5 mm. The envisaged total production for the line is about 100,000 tons/year with a process speed of 60 m/min.

The line is equipped with a double unwinding pay off reels and with a tailor-made stitcher with automatic spray lubrication system. The entry side trimmer is equipped with an integrated scrap chopper. The alkali degreasing section is made by a spray tunnel with multistage cascade rinsing section. Entry and exit loopers are horizontal type with double winch motorization.

The chemical process starts with an acid tunnel etching section, followed by a no-rinse spray titanium zirconium passivation and a squeegee roll coater for oxylane product for automotive adhesive bonding application.

The exit side includes a tension leveler, a pre-aging furnace, an automatic surface inspection system, a dry lube smelter, and a rotary shear. The thermal portion is supplied by EBNER Industrieofenbau GmbH, one of the leading suppliers in floating furnaces for aluminum heat-treatment processing line plant, consolidating the partnership between the two companies in aluminum lines and increasing their top record reference list worldwide.

The line is expected to start its production at the beginning of 2021.

“This new order confirms Tenova as a reliable partner in processing lines for aluminum thanks to our continuous effort to improve the design and the manufacture of its supply to maximize line availability,” said Nicola Cavero, Tenova senior vice president Italimpianti & Strip Processing. “We were chosen among several companies and are very proud of this new contract that consolidates our leadership in this field.”

More information: www.tenova.com