Some unique features of the Endocarb System:

  • The Endocarb System is easily programmed using an oxygen probe
  • The effective case depth is reached over 30% faster than conventional carburizing
  • The Endocarb System uses less than 1/2 of the natural gas of a conventional process
  • Unlike conventional carburizing, a very low flow of atmosphere is required
  • Very little time is required to establish a 1.45% CP on heat up after shut down
  • “Plunge Cooling” - Will cool the load down from carburizing temperature to quench temperature much faster by flowing 100% blower air and 0% gas into the furnace burner
  • A sharper drop off in carbon at the effective case depth for a more ductile core
  • No endogas from an outside generator is required in the furnace hot zone
  • Work loads using this system are always clean
  • Atmosphere gas from the endocarb enters the furnace just under 1,825˚F reacted
  • Carbon potential will operate from under .40 to 1.45% CP
  • Pay back for this system can be less than six months because of shorter cycles
  • No catalyst to change as the endocarb unit is self catalytic
  • User friendly and very easy to operate
  • An unsafe condition will shut down the system and sound an alarm
  • Long trouble free life can be expected
  • System will operate trouble free with very little maintenance